Nylon 12 (Polyamide)

PA12

ENTHUSIAST Flexible, tough nylon for mechanical parts

PA12 is unfilled nylon — the flexible, fatigue-resistant cousin of PA-CF. Where PA-CF is stiff, PA12 bends and recovers. It's the right choice for parts that need to flex repeatedly without breaking — hinges, cable strain reliefs, living hinges, snap fits. Requires enclosure and active drying.

Print Settings
Nozzle Temp 240–260°C
Bed Temp 70–90°C
Chamber 45–55°C recommended
Cooling Fan 20–40%
Max Speed 60 mm/s
Heat Deflection ~110°C
Difficulty Intermediate
Updated 2026-05-31
At a glance
Pros
  • Excellent fatigue resistance — handles repeated flex cycles without cracking
  • Self-lubricating surface — ideal for gears, cams, and bearing surfaces
  • High heat resistance (~110°C)
  • Good chemical resistance
  • Tough and impact resistant
Cons
  • Extreme moisture sensitivity — must be dried and stored carefully
  • Enclosure required
  • Warps without proper chamber temperature
  • Slower print speeds than PLA or PETG
  • More expensive than most engineering alternatives
Overview

PA12 is unfilled nylon: not the rigid, stiff material that PA-CF gives you, but the flexible, resilient one. Where carbon-filled nylon resists deflection, PA12 bends and springs back. That makes it the correct material for living hinges, snap fits, cable management parts, and anything that needs to survive thousands of flex cycles without fatigue cracking.

The self-lubricating surface is a real advantage. Nylon gears run against nylon or metal surfaces with very low friction and no need for added lubrication. If you’re building a printer part that moves against another part repeatedly, PA12 is worth the extra setup complexity over PETG.

That complexity is real. Moisture is the central problem: nylon absorbs water from the air faster than almost any other filament and the resulting prints are bubbly, weak, and dimensionally inconsistent. Dry every spool at 70°C for eight hours before printing and print from an active dryer. Enclosure temperature of 45–50°C is required — cold chamber means warping, full stop. Get those two things right and PA12 is a reliable, repeatable material that unlocks part geometries nothing else can handle.

Brand Recommendations
Polymaker PA12-CF TOP
$44.99/kg

Actually PA12 with light CF loading — stiffest of the PA12 options while retaining flexibility. Best all-rounder.

Prusament PA11 CF TOP
$59.99/kg

Bio-based PA11 — less moisture absorption than PA12. Most forgiving nylon to print. Worth the premium.

Fiberon PA12 MID
$34.99/kg

Good value unfilled PA12. More moisture sensitive than premium options. Dry before every print.

Troubleshooting
Warping
Cause Nylon shrinkage without enclosure heat
Fix Sealed enclosure at 50°C. Garolite bed surface best for nylon. Large brim on wide flat parts.
Moisture failures
Cause Nylon absorbs moisture very fast — faster than PETG
Fix Dry at 70°C for 8 hours. Print from active dryer. Never leave open overnight.
Layer delamination
Cause Too much cooling fan slows layer bonding
Fix Reduce fan to 20%. Increase perimeter overlap. Slow down to 50mm/s.
Printer Compatibility
Printer Rating Notes
Voron 2.4 EXCELLENT Enclosed chamber at 50°C. Nevermore filter recommended.
Bambu X1C / P1S EXCELLENT AMS Lite compatible. Chamber heat helps considerably.
RatRig V-Core 3 EXCELLENT Enclosed. Chamber heater recommended.
Bambu A1 / A1 Mini POOR No enclosure. Warping will ruin most prints.
Prusa MK4 POOR Open frame. Only viable with a full enclosure mod.